Mechanical Properties Metric English Comments
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Network Polymers Kepital® F20-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Network Polymers Kepital® F40-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Niche Polymer PCABSN8BK PC/ABS
Information provided by Niche Polymer
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP2-[color]-3 Acetal Copolymer, Medium Flow, General Purpose Molding, UV Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength at Break 61.4 MPa

@Thickness 50.8 mm
8900 psi

@Thickness 2.00 in
ASTM D638
Teknor Apex Synres® PP G15 18 Polypropylene, Glass Reinforced
Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many ..
Tensile Strength at Break 61.4 MPa
8900 psi
Abatron AboCast 8504-5 One-Component Epoxy
AboCast 8504-5 is a clear, plasticized one-component epoxy system with very high strength and impact. It provides exceptional physical properties and thermal shock resistance from sub-zero to modera..
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength  (Unverified Data**)
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Walled Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength at Break 61.4 MPa
8900 psi
ASTM D638
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.