Material Notes:
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.85 g/cc
0.284 lb/in³
Typical Carbon Steel
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 386 MPa
56000 psi
71.0 MPa

@Temperature 649 °C
10300 psi

@Temperature 1200 °F
105 MPa

@Temperature 538 °C
15200 psi

@Temperature 1000 °F
143 MPa

@Temperature 538 °C
20700 psi

@Temperature 1000 °F
Tensile Strength, Yield 324 MPa
47000 psi
55.8 MPa

@Temperature 649 °C
8090 psi

@Temperature 1200 °F
Elongation at Break 34 %
34 %
Modulus of Elasticity 201 GPa
29200 ksi
88.3 GPa

@Temperature 649 °C
12800 ksi

@Temperature 1200 °F
183 GPa

@Temperature 316 °C
26500 ksi

@Temperature 600 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air >= 677 °C
>= 1250 °F