Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Plaskolite Optix® CA-75 General Purpose Acrylic Resin
Injection Molding and Extrusion Grade Pellets. Highest heat resistance, medium flow.
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ISO value at 5mm/min.
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
Polycasa Acryl® G 77 E Acrylic, Extrusion Grade
Extrusion grade for semi-finished products such as profile, sheet and tubes; TV-, HiFi - and video-windows.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1200-10 Polycarbonate Resin
Description: LUPOY PC 1200-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1201-15 Polycarbonate Resin
Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1301-10 Polycarbonate Resin
Description: LUPOY PC 1301-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1301-12 Polycarbonate Resin
Description: LUPOY PC 1301-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy NF1007F 10R Polycarbonate Resin
Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Lucky CG-920 Acrylic
May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability.
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Lucky EG-930 Acrylic, Injection Grade
Injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Lucky IG-840 Acrylic, Injection Grade
General purpose injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and col..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1300-12 Polycarbonate Resin
Description: LUPOY PC 1300-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1302-10 Polycarbonate Resin
Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1303AH-10 Polycarbonate Resin
Description: LUPOY PC 1303AH-10 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and ..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM Data
Styron CALIBREâ„¢ 200 10 Polycarbonate, General Purpose
CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins ..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM Data
Styron CALIBREâ„¢ 2060 15 Polycarbonate, Sterilization Grade
CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clari..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 2061-15 Polycarbonate
CALIBREâ„¢ 2061-15 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM Data
Styron CALIBREâ„¢ 300 10 Polycarbonate, General Purpose
CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Styron CALIBREâ„¢ 301-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM Data
Styron CALIBREâ„¢ MEGARAD 2080 10 Polycarbonate, Gamma Radiation Resistant
CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4330-10 Polycarbonate
EMERGEâ„¢ PC 4330-10 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Styron CALIBREâ„¢ 303-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Ultimate 71.0 MPa
10300 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4310-15 Polycarbonate
EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4510-10 Polycarbonate
EMERGEâ„¢ PC 4510-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4530-15 Polycarbonate
EMERGEâ„¢ PC 4530-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
Cotronics Duralco™ 4460 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant
Excellent adhesion to metals, plastics, ceramics and glass. High bond strength, low moisture absorption, high thermal stability, low shrinkage and excellent chemical, electrical, and radiation resi..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Cast Nylons Nycast® 6MPB Plasticized Nylon 6
A plasticized Type 6 material, NYCAST® 6MPB is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese..
Tensile Strength, Ultimate 71.0 MPa

@Temperature 649 °C
10300 psi

@Temperature 1200 °F
AK Steel Aluminized Carbon Steel, Commercial Steel (CS Type B), Standard Grade
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direc..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Asahi Kasei Delpet® 60N Acrylic Molding Compound
60N is a medium grade of heat resistance and mechanical strength, allowing injection molding through relatively small gates and runners. General Delpet® qualities include attractive transparency, ..
Copyright © lookpolymers.com All Rights Reserved