Maximum Service Temperature, Air 677 °C
1250 °F
Upper limit of working range
Heatbath/Park #800 High Speed Hardening Salt
Working range covers temperatures frequently used in hardening and tempering steel. This product is also used as a high speed quench and draw.Information provided by Heatbath Corporation - Park Met..
Maximum Service Temperature, Air 677 °C
1250 °F
Upper limit of working range
Heatbath/Park #800 High Speed Hardening Salt
Working range covers temperatures frequently used in hardening and tempering steel. This product is also used as a high speed quench and draw.Information provided by Heatbath Corporation - Park Met..
Maximum Service Temperature, Air 677 °C
1250 °F
Upper limit of working range
Heatbath/Park #800 Neutral Salt
Working range covers temperatures frequently used in hardening and tempering steel. This product is also used as a high speed quench and draw.Information provided by Heatbath Corporation - Park Met..
Maximum Service Temperature, Air 677 °C
1250 °F
Upper limit of working range
Heatbath/Park #800 Quenching and Tempering Salt
Working range covers temperatures frequently used in hardening and tempering steel. This product is also used as a high speed quench and draw.Information provided by Heatbath Corporation - Park Met..
Maximum Service Temperature, Air 677 °C
1250 °F
Recommended Operating Temperature
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator
Fiberfrax Fibermat is a lightweight, high-strength needled insulating blanket. The blanket fibers are spun from a ceramic composition having a normal use limit of 760°C (1400°F). Fibermat is com..
Maximum Service Temperature, Air 677 °C
1250 °F
Bales Mold Service Nibore® Electroless Nickel - Boron Nitride Mold Coating
Nibore® is an electroless nickel phosphorus coating that incorporates boron nitride particles in a co-deposited nickel matrix. This unique process is formulated to produce a uniformly dispersed bor..
Maximum Service Temperature, Air >= 677 °C
>= 1250 °F
AK Steel ASTM A 463 / SAE J1392 040 AHK, Grade 40 Aluminized Carbon Steel, Structural Steel (SS)
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate.Information provided by AK Steel
Maximum Service Temperature, Air >= 677 °C
>= 1250 °F
AK Steel SAE J1392 050 XLK, Grade 50 Aluminized Carbon Steel, High Strength Low Alloy Steel (HSLAS)
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate.Information provided by AK Steel
Maximum Service Temperature, Air 677 °C
1250 °F
oxidation resistance is good in continuous service
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600)
Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties..
Maximum Service Temperature, Air 677 °C
1250 °F
oxidation resistance is good in continuous service
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 593°C (UNS S41600)
Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties..
Maximum Service Temperature, Air 677 °C
1250 °F
oxidation resistance is good in continuous service
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 649°C (1200°F) (UNS S41600)
Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties..
Maximum Service Temperature, Air >= 677 °C
>= 1250 °F
AK Steel Aluminized Carbon Steel, Commercial Steel (CS Type B), Standard Grade
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direc..
Maximum Service Temperature, Air >= 677 °C
>= 1250 °F
AK Steel Aluminized Carbon Steel, Deep Drawing Steel (DDS Type B), Standard Grade
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. DDS is made by adding aluminum to the molten steel and..
Maximum Service Temperature, Air >= 677 °C
>= 1250 °F
AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. Interstitial Free (I-F) steels are made by adding tita..
Maximum Service Temperature, Air >= 677 °C
>= 1250 °F
AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. Interstitial Free (I-F) steels are made by adding tita..
Maximum Service Temperature, Air 677 °C
1250 °F
oxidation resistance is good in continuous service
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 760°C (UNS S41600)
Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties..
Maximum Service Temperature, Air 677 °C
1250 °F
oxidation resistance is good in continuous service
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 538°C (UNS S41600)
Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties..
Maximum Service Temperature, Air 677 °C
1250 °F
oxidation resistance is good in continuous service
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 704°C (UNS S41600)
Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties..