Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 10300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ISO value at 5mm/min.
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Plaskolite West Optix® CA-75 General Purpose Acrylic Resin
Injection Molding and Extrusion Grade Pellets. Highest heat resistance, medium flow.
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1201-15 Polycarbonate Resin
Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Lucky CG-920 Acrylic
May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability.
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Lucky EG-930 Acrylic, Injection Grade
Injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Lucky IG-840 Acrylic, Injection Grade
General purpose injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and col..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1300-10 Polycarbonate Resin
Description: LUPOY PC 1300-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1302-10 Polycarbonate Resin
Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin
Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1303-10 Polycarbonate Resin
Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1303AH-10 Polycarbonate Resin
Description: LUPOY PC 1303AH-10 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and ..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
LG Chemical Lupoy 1303AH-15 Polycarbonate Resin
Description: LUPOY PC 1303AH-15 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and ..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM Data
Styron CALIBREâ„¢ 200 10 Polycarbonate, General Purpose
CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins ..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM Data
Styron CALIBREâ„¢ 2060 10 Polycarbonate, Sterilization Grade
CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clari..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM Data
Styron CALIBREâ„¢ 300 15 Polycarbonate, General Purpose
CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Styron CALIBREâ„¢ 301-10 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Styron CALIBREâ„¢ 301-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM Data
Styron CALIBREâ„¢ MEGARAD 2080 10 Polycarbonate, Gamma Radiation Resistant
CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4310-10 Polycarbonate
EMERGEâ„¢ PC 4310-10 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4330-15 Polycarbonate
EMERGEâ„¢ PC 4330-15 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4510-15 Polycarbonate
EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4530-10 Polycarbonate
EMERGEâ„¢ PC 4530-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Styron CALIBREâ„¢ 303-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Ultimate 71.0 MPa
10300 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4310-15 Polycarbonate
EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4510-10 Polycarbonate
EMERGEâ„¢ PC 4510-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
DIN 53504
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Cast Nylons Nycast® 6MPB Plasticized Nylon 6
A plasticized Type 6 material, NYCAST® 6MPB is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese..
Tensile Strength, Ultimate 71.0 MPa

@Temperature 649 °C
10300 psi

@Temperature 1200 °F
AK Steel Aluminized Carbon Steel, Commercial Steel (CS Type B), Standard Grade
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direc..
Tensile Strength, Ultimate 71.0 MPa
10300 psi
ASTM D638
Asahi Kasei Delpet® 60N Acrylic Molding Compound
60N is a medium grade of heat resistance and mechanical strength, allowing injection molding through relatively small gates and runners. General Delpet® qualities include attractive transparency, ..
Copyright © lookpolymers.com All Rights Reserved