Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 55.8 MPa @Temperature 23.0 °C |
8090 psi @Temperature 73.4 °F |
ASTM D638 |
PolyOne Geon™ CPVC MC250 Polyvinyl Chloride, Chlorinated (CPVC) The Geon MC250 CPVC is an injection molding fittings compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geo.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8090 psi | ASTM D638 |
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 55.8 MPa | 8090 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ IM 401-11 Polycarbonate Resin Overview: CALIBREâ„¢ IM 401-11 Impact Modified Polycarbonate resin is available in opaque formulations that offer benefits ranging from superior low temperature impact strength to easy process wi.. |
|||
Tensile Strength, Yield | 55.8 MPa | 8090 psi | ASTM Data |
Styron CALIBRE™ IM 401 11 Polycarbonate, Impact Modified CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM401 polycarbonate resins exhibit an excellent balance of impact strength and.. |
|||
Tensile Strength, Yield | 55.8 MPa @Temperature 649 °C |
8090 psi @Temperature 1200 °F |
|
AK Steel Aluminized Carbon Steel, Commercial Steel (CS Type B), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direc.. |