Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 677 °C | 1250 °F | Upper limit of working range |
Heatbath/Park #800 High Speed Hardening Salt Working range covers temperatures frequently used in hardening and tempering steel. This product is also used as a high speed quench and draw.Information provided by Heatbath Corporation - Park Met.. |
|||
Maximum Service Temperature, Air | 677 °C | 1250 °F | Upper limit of working range |
Heatbath/Park #800 High Speed Hardening Salt Working range covers temperatures frequently used in hardening and tempering steel. This product is also used as a high speed quench and draw.Information provided by Heatbath Corporation - Park Met.. |
|||
Maximum Service Temperature, Air | 677 °C | 1250 °F | Upper limit of working range |
Heatbath/Park #800 Neutral Salt Working range covers temperatures frequently used in hardening and tempering steel. This product is also used as a high speed quench and draw.Information provided by Heatbath Corporation - Park Met.. |
|||
Maximum Service Temperature, Air | 677 °C | 1250 °F | Upper limit of working range |
Heatbath/Park #800 Quenching and Tempering Salt Working range covers temperatures frequently used in hardening and tempering steel. This product is also used as a high speed quench and draw.Information provided by Heatbath Corporation - Park Met.. |
|||
Maximum Service Temperature, Air | 677 °C | 1250 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator Fiberfrax Fibermat is a lightweight, high-strength needled insulating blanket. The blanket fibers are spun from a ceramic composition having a normal use limit of 760°C (1400°F). Fibermat is com.. |
|||
Maximum Service Temperature, Air | 677 °C | 1250 °F | |
Bales Mold Service Nibore® Electroless Nickel - Boron Nitride Mold Coating Nibore® is an electroless nickel phosphorus coating that incorporates boron nitride particles in a co-deposited nickel matrix. This unique process is formulated to produce a uniformly dispersed bor.. |
|||
Maximum Service Temperature, Air | >= 677 °C | >= 1250 °F | |
AK Steel ASTM A 463 / SAE J1392 040 AHK, Grade 40 Aluminized Carbon Steel, Structural Steel (SS) Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate.Information provided by AK Steel |
|||
Maximum Service Temperature, Air | >= 677 °C | >= 1250 °F | |
AK Steel SAE J1392 050 XLK, Grade 50 Aluminized Carbon Steel, High Strength Low Alloy Steel (HSLAS) Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate.Information provided by AK Steel |
|||
Maximum Service Temperature, Air | 677 °C | 1250 °F | oxidation resistance is good in continuous service |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Maximum Service Temperature, Air | 677 °C | 1250 °F | oxidation resistance is good in continuous service |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 593°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Maximum Service Temperature, Air | 677 °C | 1250 °F | oxidation resistance is good in continuous service |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 649°C (1200°F) (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Maximum Service Temperature, Air | >= 677 °C | >= 1250 °F | |
AK Steel Aluminized Carbon Steel, Commercial Steel (CS Type B), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direc.. |
|||
Maximum Service Temperature, Air | >= 677 °C | >= 1250 °F | |
AK Steel Aluminized Carbon Steel, Deep Drawing Steel (DDS Type B), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. DDS is made by adding aluminum to the molten steel and.. |
|||
Maximum Service Temperature, Air | >= 677 °C | >= 1250 °F | |
AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. Interstitial Free (I-F) steels are made by adding tita.. |
|||
Maximum Service Temperature, Air | >= 677 °C | >= 1250 °F | |
AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. Interstitial Free (I-F) steels are made by adding tita.. |
|||
Maximum Service Temperature, Air | 677 °C | 1250 °F | oxidation resistance is good in continuous service |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 760°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Maximum Service Temperature, Air | 677 °C | 1250 °F | oxidation resistance is good in continuous service |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 538°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Maximum Service Temperature, Air | 677 °C | 1250 °F | oxidation resistance is good in continuous service |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 704°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |