Mechanical Properties Metric English Comments
Tensile Strength, Yield 324 MPa
47000 psi
Pacific Sintered Materials FCC-200-P High Carbon Copper Steel Powdered Metal
High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI..
Tensile Strength, Yield 324 MPa
47000 psi
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-200-P Powdered Metal
High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP..
Tensile Strength, Yield 324 MPa

@Temperature 93.3 °C
47000 psi

@Temperature 200 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Tensile Strength, Yield 324 MPa
47000 psi
Kinetics MIM 4605 Low Alloy Steel (As Sintered)
Low alloy steel, carbon, nickel, molybdenum. A multi-purpose, economical material that offers various strength, hardness, and wear resistance properties depending if it is heat treated and the heat ..
Tensile Strength, Yield 324 MPa

@Strain 0.200 %,
Temperature 538 °C
47000 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Yield 324 - 469 MPa
47000 - 68000 psi
0.2% offset
Eagle Brass 510 Phosphor Bronzes 5% A, 1/2 Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Yield 324 MPa
47000 psi
Chicago Extruded Metals BioBrass® UNS C27450 Copper-Zinc Alloy
Finished product available as wire or tube.Chicago Extruded Metal temper code: H04Information provided by Chicago Extruded Metals
Tensile Strength, Yield 324 MPa

@Temperature 482 °C
47000 psi

@Temperature 900 °F
Dura-Bar 65-45-12 HRDS Continuously Cast Ductile Iron Bar Stock ASTM A536
Dura-Bar 4512 HRDS is a high-silicon ductile iron intended for use at elevated temperatures or when a part is subjected to thermal cycling, such as permanent mold applications. The ferritic structu..
Tensile Strength, Yield 324 MPa
47000 psi
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy
Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening..
Tensile Strength, Yield 324 MPa
47000 psi
AK Steel Aluminized Carbon Steel, Commercial Steel (CS Type B), Standard Grade
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. May be moderately formed. A specimen cut in any direc..
Tensile Strength, Yield 324 MPa

@Strain 0.200 %,
Temperature 538 °C
47000 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Tensile Strength, Yield 324 MPa

@Strain 0.200 %
47000 psi

@Strain 0.200 %
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Tensile Strength, Yield 324 MPa

@Strain 0.200 %
47000 psi

@Strain 0.200 %
Haynes Hastelloy® G-30® alloy, 19.1 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..