Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer A. Schulman, Inc.
Trade Name POLYTROPE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temperatures. TPP 503 is UV stable, paintable and pigmentable.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
Melt Index of Compound 9.0 g/10 min
9.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Yield 13.8 MPa
2000 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 0.310 GPa
45.0 ksi
ASTM D790
Gardner Impact 36.0 J

@Temperature -30.0 °C
26.6 ft-lb

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Brittleness Temperature -50.0 °C