Material Notes:
The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh environment. Descriptions Bars: Aluminum alloy Screws: Inox A2Threaded insert: Stainless steelStandard treatment: SurTec 650Information provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 - 300 °C
356 - 572 °F
Descriptive Properties Value Comments
Damping Factor 0.1 - 0.2
F, Max Dynamic 1255 daN
45.0 mm, up
250.0 daN
102.0 mm, 45° down and out
375.0 daN
70.0 mm, left and right
400.0 daN
68.0 mm, down
417.0 daN
67.3 mm, up and down
F, Max Static 100.0 daN
22.5 mm, 45° down and out
135.0 daN
12.5 mm, down
135.0 daN
10 mm, up
67.0 daN
22.1 mm, up and down
67.0 daN
24.0 mm, left and right
Transmissibility at resonance 3