Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 261R PC (Europe-Africa-Middle East) LEXAN 261R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 263R PC (Europe-Africa-Middle East) LEXAN 263R is a medium viscosity multi purpose UV stabilized grade and contains release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 943X PC Copolymer (Asia Pacific) Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Asia Pacific) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE4472L PC (Asia Pacific) Lexan* FXE4472L is a 20% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Asia Pacific) Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® PC1000 PC (Europe-Africa-Middle East) PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 2.16 kg, Temperature 260 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C7230P PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polykemi AB POLYform POM C M90 Polyoxymethylene Information provided by Polykemi AB |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD4472 PC (Europe-Africa-Middle East) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML3999 PC (Europe-Africa-Middle East) LEXAN ML3999 is a medium viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Melt Index of Compound | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICORENEâ„¢ 324-1327 LMDPE Rotational Molding Resin Description: ICORENE 324-1327 is a linear medium density polyethylene developed for use in rotational molding. It has very good flow properties allowing the material to reproduce fine detail and me.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 10.0 kg, Temperature 280 °C |
9.0 g/10 min @Load 22.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN3 is a 30% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Melt Index of Compound | 9.0 g/10 min | 9.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Melt Index of Compound | 9.0 g/10 min | 9.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Melt Index of Compound | 9.0 g/10 min | 9.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Melt Index of Compound | 9.0 g/10 min | 9.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTADER® 4403 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4403 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER 4403 is a versatile adhesive for extrusion lamination, de.. |
|||
Melt Index of Compound | 9.0 g/10 min | 9.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD4471 PC (Europe-Africa-Middle East) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |