ChevronTexaco Soluble XL

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Soluble
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Soluble XL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Soluble Oil XL delivers value through:No separation — Excellent emulsion even with hard waterRust protection for steel work and machined parts even when water-oil emulsion ratios are eighty to oneAbility to control bacterial growth and rancid odorsCooling improved by metal wetting. Also good chip settling.Reduced foaming — Possibility of sump overflow minimized.Stability in storage — Will not turn rancid.Texaco Soluble Oil XL is an emulsifying oil which readily mixes with water, forming a homogeneous and exceptionally stable emulsion. It provides rust and corrosion inhibition and foam inhibition. It is used in the machining of both ferrous and nonferrous metals, particularly when cutting with carbon or high speed steel or tungsten carbide tools. It also combats bacterial growth in machine sumps.Texaco Soluble Oil XL is used broadly in machine shop operations as a multifunctional cutting fluid. It is designed primarily to cool and lubricate the contact point of the tool and the work piece. It also prevents rusting or corrosion of the metals being machined as well as controls growth of bacteria, which is a constant problem in soluble oil circulating systems due to outside contamination.Texaco Soluble Oil XL minimizes surface foam and speeds the release of entrained air which could cause pump cavitation. This is a versatile fluid designed to meet many of the situations encountered in the metalworking industry.Texaco Soluble Oil XL is recommended for all metals (except magnesium) where maximum cooling is desired, particularly when cutting with carbon, high speed steel, or tungsten carbide tools.Texaco Soluble Oil XL is used extensively in milling, drilling, gear cutting, turning, planing, shaping, sawing, and grinding operations.One gallon of Texaco Soluble Oil XL for each 20 gallons of water satisfies most cutting operations; however, the add oil to water to avoid forming sticky invert emulsions which do not emulsify properly in water. See the Soluble Oil Mixing Recommendations chart for the proper ratio for the application.Texaco Soluble Oil XL is suitable for use in automotive cooling systems to prevent rust and corrosion. A mixture of forty to one is most often used. However, always follow engine manufacturers recommendations. It is preferable to mix radiator water and oil in a separate container. Additions to the radiator should be made from this container. As with any other "additives", the radiator should be drained and flushed occasionally, since evaporation and leakage cause proportions to change. Do not recommend Texaco Soluble Oil XL emulsions for magnesium. Hot magnesium is a fire hazard when it contacts water. The preferred recommendation is Texaco Alcaid® 19 (ISO 22).Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.CPS Number: 221626; MSDS Number: 8951
Physical Properties Metric English Comments
API Gravity 27.7 °
27.7 °
Saybolt Viscosity at 100°F 187 SUS
187 SUS
Saybolt Viscosity at 210°F 47 SUS
47 SUS
Kinematic Viscosity at 40°C (104°F) 36.5 cSt
36.5 cSt
Kinematic Viscosity at 100°C (212°F) 6.3 cSt
6.3 cSt
Thermal Properties Metric English Comments
Pour Point -12.0 °C
10.4 °F
Flash Point 200 °C
392 °F
Descriptive Properties Value Comments
Fat Present