Material Notes:
Data provided by the manufacturer, ComAlloy International Company.30% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 82.0 MPa
11900 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 134 MPa
19400 psi
ASTM D790
Flexural Modulus 6.00 GPa
870 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.14 J/cm
4.01 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 - 275 °C
491 - 527 °F
Deflection Temperature at 0.46 MPa (66 psi) 251 °C
484 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 291 - 302 °C
556 - 576 °F