Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Plastcom SLOVAMID 66 GF 33 TS PA66, 33% glass fibre, thermal stability
FeaturesPA 66 for injection moulding, chemically reinforced with 33% glass fibre, heat stabilized, suitable for high strength and high impacted mouldings. Used in automotive, engineering and electri..
Density 1.39 g/cc
0.0502 lb/in³
ISO data
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is..
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
PolyOne Lubri-Tech™ PS-000/15T-2S Polyester (PBT) - 15% PTFE Lubricated - 2% Silicone Lubricated  (discontinue
Data provided by PolyOne.
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183 B
Idemitsu Kosan Xarec® EA 528 SPS, 30% Glass Filled  (discontinued **)
Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications
Density 1.39 - 1.61 g/cc
0.0502 - 0.0582 lb/in³
Average value: 1.50 g/cc Grade Count:17
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an..
Density 1.39 g/cc
0.0502 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp AF008 ABS
LNP* Thermocomp* AF008 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK (Asia Pacific)
LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP PX85100 PA 6
LNP* THERMOCOMP* PX85100 is a compound based on Nylon 6 resin containing Proprietary Filler(s).
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Techmer ES Electrablend® PA6 GF20 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight/Unspecified Filler/Reinfor.Additive: LubricantFeatures: Conductive and LubricatedAppear..
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Tipco Tipcolite® TMS 311 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength
Medium Flow Phenolic Compound, Reinforced with Cotton, Filler & Wood FlourApplications: Industrial & AutomotivesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr..
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Chengdu Polyster FH2040 Thermoplastic Polyether-ester Elastomer (TPEE)
Blend of H2040 and self-made flame retardant material. Excellent flex resistance at low temperatures. Excellent flex-fatigue resistance. Applications requiring flexibility at low temperatures and fl..
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
DSM Arnitel® PL460-S 46 Shore D Copolyester Elastomer, Injection Grade (Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Density 1.39 g/cc
0.0502 lb/in³
dry; ISO 1183
DSM EcoPaXX® Q-X07209 PA410-I-GF40
% Glass Reinforced, Impact Modified
Density 1.39 g/cc
0.0502 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
Density 1.39 g/cc
0.0502 lb/in³
DuPont Teijin Films Melinex® ST730 Polyester Film
Melinex® ST730 is an optically clear, heat stabilized polyester film which is differentially treated on both sides. One side provides exceptional adhesion to both solvent based and UV curing inks a..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® EL Polyester Film, 142 Gauge
Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® LJP Polyester Film, 700 Gauge
Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® MDA Polyester Film, 1000 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® OL2 Polyester Film, 100 Gauge
Product Description: Mylar® OL2 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and f..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® RSX Polyester Film, 500 Gauge
Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® RSX951 Polyester Film, 105 Gauge
Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 300 Gauge
Mylar® type WC11 films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectric and good handlin..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® LJP Polyester Film, 92 Gauge
Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider us..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® MDA Polyester Film, 300 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® MDA Polyester Film, 500 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Celanese Celcon® LU-02 POM, UV Resistant
Celcon® acetal copolymer grade LU-02 is UV stabilized material displaying a reduced gloss over standard UV acetal grades.UV resistant, reduced glossStandard reciprocating screw injection molding ma..
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Celanese Hostaform® S 27063 XAP2® POM
Description: Easy flowing elastomer-containing injection molding type based on HOSTAFORM C 27021; with higher impact strength and reduced emissions. Burning rate ISO 3795 and FMVSS 302 < 100 mm/min ..
Density 1.39 g/cc
0.0502 lb/in³
A. Schulman ComAlloy Hiloy® 518 Polycarbonate, Carbon Fiber Reinforced
Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Celanese Hostaform® S 27072 WS 10/1570 POM, Impact Modified  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POM-HIEasy flowing, elastomer-containing injection molding grade; black; weathering resistantInformation provided by Celanese
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Celanese Celcon® TX90 Acetal Copolymer
An M90 based material tailored to provide moderate improvement in impact strength and flexibility.Information provided by Celanese Corporation.
Copyright © lookpolymers.com All Rights Reserved