Spartech M60480 General Purpose PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech M60480 General Purpose PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. Best for filled moldings, tool handles, and household products.Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
+.02
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
10 sec ± 3
Tensile Strength, Yield 16.3 MPa
2370 psi
Elongation at Break 345 %
345 %
100% Modulus 0.00896 GPa
1.30 ksi
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F