A. Schulman ComAlloy E-17099B Nylon 6/6, Electrically Conductive - Carbon Fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Conductive
Manufacturer A. Schulman ComAlloy
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy E-17099B Nylon 6/6, Electrically Conductive - Carbon Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 145 MPa
21000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 14.0 GPa
2030 ksi
ASTM D790
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
500 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 10.0 - 100 ohm-cm
10.0 - 100 ohm-cm
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05