Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Aqualoy® 140 Polypropylene, Glass Reinforced, Chemically Coupled NSF

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer A. Schulman ComAlloy
Trade Name Aqualoy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Aqualoy® 140 Polypropylene, Glass Reinforced, Chemically Coupled NSF.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability and high strength traits into a unique property blend.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Ultimate 76.0 MPa
11000 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 112 MPa
16200 psi
ASTM D790
Flexural Modulus 5.50 GPa
798 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.57 J/cm
12.3 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 164 °C
327 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 151 °C
304 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 229 - 246 °C
444 - 475 °F