Multibase Multi-Flamâ„¢ 0206 PP Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Flam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flamâ„¢ 0206 PP Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Flame RetardantHalogen Content, Low to None Forms:PelletsUses:TubingWire JacketingFurnitureInformation provided by Multibase
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Break 480 %
480 %
ASTM D638
Flexural Modulus 1.08 GPa
157 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
0.125 in