Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kleerdex Vinyloy™ 100 Acrylic/PVC Thermoplastic Sheet  (discontinued **)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kleerdex Vinyloy™ 100 Acrylic/PVC Thermoplastic Sheet  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Utility gradeApplications: Vinyloy 100 sheet is a fire retardant that can be used to substitute effectively for ABS and other utility grade thermoplastics.Features: Vinyloy 100 sheet is a recycled grade of proprietary acrylic/PVC thermoplastic sheet that is cost competitive with other utility grades of thermoplastic sheet while offering improved performance. Vinyloy 100 sheet is UL recognized 94 V-0 and 5V.Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
ASTM D785
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D638
Modulus of Elasticity 2.068 GPa
299.9 ksi
Flexural Yield Strength 63.0 MPa
9140 psi
ASTM D790
Izod Impact, Notched 4.27 J/cm

@Temperature 23.0 °C
8.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
annealed; ASTM D648
Flammability, UL94 V-0
V-0
V-0, 5V; UL Standard 94
Processing Properties Metric English Comments
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature
Users viewing this material also viewed the following: