Polymer Property : Flexural Strength = 112 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 112 MPa
16200 psi
Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Flexural Strength 112 MPa
16200 psi
Poco Graphite ZXF-5Q Industrial Grade Graphite
SSH hardness is 86.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p..
Flexural Strength 112 MPa
16200 psi
ASTM D790
Polymer Resources PC-G20-[color]-WS Polycarbonate, 20% Glass Reinforced
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Strength 112 MPa
16200 psi
ASTM D 790
NOVA Chemicals Dylark® FG7200 High-Heat Styrenic Copolymer
Product Description and Features: Styrene/maleic anhydride copolymer with high-heat resistance and high modulus. Resins designed for use in foam extrusion.Processing: Contact NOVA Chemicals techn..
Flexural Strength 112 MPa
16200 psi
ISO 178
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro..
Flexural Strength 112 MPa
16200 psi
ISO 178
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation..
Flexural Strength 112 MPa
16200 psi
2mm/min; ASTM D790
Kingfa JH720 G10 10% Glass Fiber Reinforced PC
Features:High mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanner cabinetComputer plug partsCD-ROM, DVDElectri..
Flexural Strength 112 MPa
16200 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI
LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant.
Flexural Strength 112 MPa
16200 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66
LNP LUBRICOMP* RL002 is a compound based on Nylon 66 resin containing 10% PTFE. Added features of this material include: Wear Resistant.
Flexural Strength 112 MPa

@Strain 3.50 %,
Temperature 175 °C
16200 psi

@Strain 3.50 %,
Temperature 347 °F
4; ISO 178
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
Flexural Strength 112 MPa
16200 psi
ISO 178
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula..
Flexural Strength 112 MPa
16200 psi
ISO 178
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and..
Flexural Strength 112 MPa
16200 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON Lexan_JK2500 PC+ABS
LNP* Stat-kon* Lexan_JK2500 compound is a 20% carbon-fiber reinforced, nonhalogenated red phosporous-free, high-flow FR PC+ABS for EMI/RFI shielding. SE of 21 dB at 1.5 mm.
Flexural Strength 112 MPa
16300 psi
ASTM D790
Techmer ES HiFill® PA6/6 0177 B Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Flexural Strength 112 MPa
16300 psi
ASTM D790
Techmer ES Luriblend® PA6 ML2 HS BK Nylon 6
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Blac..
Flexural Strength 112 MPa
16300 psi
ASTM D790
Techmer ES Luriblend® PA6 ML3 BK Nylon 6
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(3%)Features: Good Wear Resistance, Low Friction, Heat Stabilized and LubricatedAppearance: Black..
Flexural Strength 112 MPa
16200 psi
ASTM D 790
Saint-Gobain Meldin® 1357 Thermoplastic Bearing Material
Meldin 1357 offers the lowest wear rate and coefficient of friction, which makes it the best candidate for tribological applications. In addition, its self-lubricating properties allow it to operat..
Flexural Strength 112 MPa
16200 psi
ISO 178
SABIC Innovative Plastics NORYL N300X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications.
Flexural Strength 112 MPa
16200 psi
ISO 178
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific)
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications.
Flexural Strength 112 MPa
16200 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON AE002 ABS
LNP* STAT-KON* AE002 is a compound based on ABS resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
Flexural Strength 112 MPa
16200 psi
ASTM D790
Plenco 08235 Polyester BMC, Compression Molded
PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable ..
Flexural Strength 112 MPa
16200 psi
dry; ISO 178
DSM Novamid® 1010C2 PA6
Easy Molding Grade
Flexural Strength 112 MPa
16200 psi
ASTM D790
Ensinger Hydel® PEI-7 Polyetherimide (PEI), Static Dissipative
A static dissipative polyetherimide utilizing proprietary filler technology which renders this material electrically conductive. This technology allows for good dimensional stability after machinin..
Flexural Strength >= 112 MPa
>= 16200 psi
cold bending
China-Yixing Longly Refractories Push Slab Corundum-Mullite
Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine..
Flexural Strength 112 MPa
16300 psi
ASTM D790
Asahi Kasei Thermylene® P-25FG-3809 25% Glass Fiber Reinforced
Information provided by Asahi Thermofil
Flexural Strength 112 MPa

@Temperature 120 °C
16200 psi

@Temperature 248 °F
ASTM Test
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Flexural Strength 112 MPa
16200 psi
ASTM D790
A. Schulman ComAlloy Aqualoy® 140 Polypropylene, Glass Reinforced, Chemically Coupled NSF
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an..
Flexural Strength 112 MPa
16200 psi
ASTM D790
A. Schulman ComAlloy Hiloy® 249 SAN, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Strength 112 MPa

@Temperature 175 °C
16200 psi

@Temperature 347 °F
3.5% Strain; ISO 178
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..