3M Scotch-Weld™ DP600 Concrete Repair and Self-Leveling

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ DP600 Concrete Repair and Self-Leveling.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600 is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a trigger, the components are automatically mixed and easily dispensed as a bubble-free self-leveling liquid.Information provided by 3M
Physical Properties Metric English Comments
Density 1.02 - 1.07 g/cc
0.0368 - 0.0387 lb/in³
Part B
1.14 - 1.19 g/cc
0.0412 - 0.0430 lb/in³
Part A
Brookfield Viscosity 1000 - 3000 cP
1000 - 3000 cP
Part A, CP#52 @ 100 rpm
1100 - 6000 cP
1100 - 6000 cP
Part B, CP#52 @ 100 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 70

@Time 3600 sec
70

@Time 1.00 hour
after cure
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Processing Properties Metric English Comments
Cure Time 4.00 min
0.0667 hour
Tack-Free, 10 g, 1/4" thick @ RT
60.0 min
1.00 hour
Full, 10 g. 1/4" thick @ RT
Descriptive Properties Value Comments
Appearance Clear Yellowish
Part A
Medium-Gray
Cured
Opaque Black
Part B