Thermal Properties Metric English Comments
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Parker Chomerics Tecknit Consil®-II 841 Molded Silver-Filled Silicone Elastomer
Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Parker Chomerics Tecknit Consil®-R 856 Pure Silver-Filled Silicone Elastomer
Description: CONSIL-R 856 offers the lowest durometer available for pure silver-filled elastomerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Parker Chomerics Tecknit SC-Consil® 860 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Parker Chomerics Tecknit SC-Consil® 862 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Parker Chomerics Tecknit SC-Consil® FR861 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Parker Chomerics Tecknit SC-Consil® FR862 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Retraction Temperature, TR10; ASTM D1329
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Paraplex G25
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Retraction Temperature, TR10; ASTM D1329
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with Benzoflex 9-88SG
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Retraction Temperature, TR10; ASTM D1329
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with DBP
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
JIS-K-6723
Denka REOMER G G5074 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
3M Scotch-Weld™ DP600 Concrete Repair and Self-Leveling
3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600 is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a trigg..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
3M Scotch-Weld™ DP604NS Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesive DP-604NS is a black, rapid setting, two-component polyurethane. It is packaged as 1:1 ratio liquids in a duo-pak cartridge. With the squeeze of the trigger, the ..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
3M Scotch-Weld™ MG90-77 UV Medical Grade Light Cure Adhesive
3M™ Scotch-Weld™ Medical Grade Light Cure Adhesive is a single component adhesive that cure to give clear bonds when exposed to appropriate ultraviolet or visible light. It contains a fluorescing ..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
3M 421 Lead Foil Tape
Self-wound plating tapeInformation provided by 3M
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Arlon SFT 0.012" (0.305 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: PET Product: Cured Self-Fusing Silicone Rubber Cross-Section: 1” Wide RectangularDescription: 1 inch wide, 12 mil thick x 10 yards long, Gray, Rectangular cross-sec..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
3M Scotch-Weld™ DP-5106 Control Joint Sealant
3M™ Scotch-Weld™ Control Joint Sealant DP-5106 is a self-leveling, gray, rapid setting, two-component polyurethane. It is packaged as 1:1 ratio liquids in duo-pak cartridges. With the squeeze of t..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
3M Scotch-Weld™ DP601 Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
3M Scotch-Weld™ DP601NS Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
3M Scotch-Weld™ MG250-55 UV Medical Grade Light Cure Adhesive
3M™ Scotch-Weld™ Medical Grade Light Cure Adhesive is a single component adhesive that cure to give clear bonds when exposed to appropriate ultraviolet or visible light. It contains a fluorescing ..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Parker Chomerics Tecknit SC-Consil® 861 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
continuous
Chesterton 860 Moldable Polymer Gasketing
Description: Chesterton® 860 Moldable Polymer Gasketing is a solid flexible gasketing material which fills in surface irregularities, stop leaks and never sticks to surfaces after curing. It is the..
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
See Note 1.