Physical Properties Metric English Comments
Brookfield Viscosity 2000 - 6000 cP
2000 - 6000 cP
DOP 60phr; ASTM D1824
LG Chemical PB1202 PVC
General Description: PB1202, homopolymer made by micro-suspension seeded polymerization, PVC Resin has a fluid property similar to Newtonian fluidity (low-viscosity) It is mainly used for non-foamin..
Brookfield Viscosity 400 - 6000 cP

@Temperature 25.0 °C
400 - 6000 cP

@Temperature 77.0 °F
25% solution in Toluene
Sibur DST-30R-01 2nd Group Styrene-Butadiene-Styrene Block Copolymer (SBS-TPE)
Kraton D 1184, 1186. As modifiers for bitumen for production of roofing materials, footwear compositions, adhesives, and coverings, as well as for modification of plastics. Addition of thermal ela..
Brookfield Viscosity 1100 - 6000 cP
1100 - 6000 cP
Part B, CP#52 @ 100 rpm
3M Scotch-Weld™ DP600 Concrete Repair and Self-Leveling
3M™ Scotch-Weld™ Concrete Repair Self-Leveling DP600 is a gray, rapid setting, two component polyurethane. It is packaged as a 1:1 ratio liquid in a duo-pack cartridge. With the squeeze of a trigg..
Brookfield Viscosity 1100 - 6000 cP
1100 - 6000 cP
Part B, CP #52 @ 100 rpm
3M Scotch-Weld™ DP601 Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon..
Brookfield Viscosity 5000 - 6000 cP
5000 - 6000 cP
Base, RVF #6 sp @ 20 rpm
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..