3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 28 - 32 %
28 - 32 %
Brookfield Viscosity 900 - 1500 cP
900 - 1500 cP
RVF #2 sp @ 20 rpm @ 80°F
Mechanical Properties Metric English Comments
Shear Strength 0.469 MPa

@Temperature 82.0 °C,
Time 1.81e+6 sec
68.0 psi

@Temperature 180 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
2.60 MPa

@Temperature 24.0 °C,
Time 1.81e+6 sec
377 psi

@Temperature 75.2 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
Peel Strength 1.05 kN/m

@Temperature 24.0 °C,
Time 86400 sec
6.00 pli

@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
1.75 kN/m

@Temperature 24.0 °C,
Time 259000 sec
10.0 pli

@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
2.45 kN/m

@Temperature -34.0 °C,
Time 1.81e+6 sec
14.0 pli

@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
3.86 kN/m

@Temperature 82.0 °C,
Time 1.81e+6 sec
22.0 pli

@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
4.21 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
24.0 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
4.21 kN/m

@Temperature 24.0 °C,
Time 432000 sec
24.0 pli

@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
5.26 kN/m

@Temperature 24.0 °C,
Time 1.81e+6 sec
30.0 pli

@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
5.61 kN/m

@Temperature 24.0 °C,
Time 605000 sec
32.0 pli

@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
5.61 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
32.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
Thermal Properties Metric English Comments
Flash Point -26.0 °C
-14.8 °F
TCC
Descriptive Properties Value Comments
Appearance Yellow
Base Polychloroprene