Polymer Property : Peel Strength = 3.86 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 3.86 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
22.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
3M Scotch-Weld™ 10 Neoprene Contact Adhesive
3M™ Scotch-Weld™ Neoprene Contact Adhesive 10 is a multi-purpose contact adhesive which may be used to bond plastic laminate, aluminum, steel, wallboard, wood, masonry, rubber and canvas.Informati..
Peel Strength 3.86 kN/m

@Temperature 82.0 °C,
Time 1.81e+6 sec
22.0 pli

@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive
Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information..
Peel Strength 3.86 kN/m

@Temperature -34.0 °C,
Time 1.81e+6 sec
22.0 pli

@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 4475 Industrial Adhesive
Features: Dries quickly to a firm bondExcellent resistance to water, plasticizer migration, many detergent and soap solutions, oils and greasesA general purpose adhesive for bonding most vinyls, cer..
Peel Strength 3.86 kN/m

@Temperature 24.0 °C,
Time 259000 sec
22.0 pli

@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
3M Scotch-Weld™ 4799 Industrial Adhesive
3M™ Scotch-Weld™ Industrial Adhesive 4799 can be used to bond most EPDM rubber, sponge rubber, rubber sheeting, felt, canvas, linoleum and other lightweight materials to many metals, woods, concre..