Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.05 kN/m @Temperature 24.0 °C, Time 86400 sec |
6.00 pli @Temperature 75.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information.. |
|||
Peel Strength | 1.05 kN/m @Temperature 23.0 °C |
6.00 pli @Temperature 73.4 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 1.05 kN/m @Temperature 23.0 °C |
6.00 pli @Temperature 73.4 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |