Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.75 kN/m @Temperature 66.0 °C, Time 1.81e+6 sec |
10.0 pli @Temperature 151 °F, Time 504 hour |
canvas/canvas |
3M Fastbond™ 30-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Peel Strength | 1.75 kN/m @Temperature 82.0 °C, Time 1.81e+6 sec |
10.0 pli @Temperature 180 °F, Time 504 hour |
canvas/canvas |
3M Fastbond™ 30-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Peel Strength | 1.75 kN/m @Temperature 24.0 °C, Time 86400 sec |
10.0 pli @Temperature 75.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 10 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 10 is a multi-purpose contact adhesive which may be used to bond plastic laminate, aluminum, steel, wallboard, wood, masonry, rubber and canvas.Informati.. |
|||
Peel Strength | 1.75 kN/m @Temperature 24.0 °C, Time 259000 sec |
10.0 pli @Temperature 75.2 °F, Time 72.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information.. |
|||
Peel Strength | 1.75 kN/m @Temperature 24.0 °C, Time 86400 sec |
10.0 pli @Temperature 75.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 5 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 5 is a sprayable contact adhesive which may be used to bond many high-pressure plastic laminates to wood, particle-board, metal and other surfacesInforma.. |
|||
Peel Strength | 1.75 kN/m @Temperature 49.0 °C |
10.0 pli @Temperature 120 °F |
180° |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Peel Strength | 1.75 kN/m @Temperature 66.0 °C, Time 1.81e+6 sec |
10.0 pli @Temperature 151 °F, Time 504 hour |
canvas/canvas |
3M Fastbond™ 30H-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Peel Strength | 1.75 kN/m @Temperature 82.0 °C, Time 1.81e+6 sec |
10.0 pli @Temperature 180 °F, Time 504 hour |
canvas/canvas |
3M Fastbond™ 30H-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Peel Strength | 1.75 kN/m @Temperature 24.0 °C |
10.0 pli @Temperature 75.2 °F |
180°, Canvas/Steel |
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov.. |