Polymer Property : Peel Strength = 6.00 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.05 kN/m

@Temperature 24.0 °C,
Time 86400 sec
6.00 pli

@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive
Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information..
Peel Strength 1.05 kN/m

@Temperature 23.0 °C
6.00 pli

@Temperature 73.4 °F
Adhesion on Aluminum; ASTM D3330
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..
Peel Strength 1.05 kN/m

@Temperature 23.0 °C
6.00 pli

@Temperature 73.4 °F
Adhesion on Aluminum; ASTM D3330
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape
3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment..