Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 1200 - 1500 cP | 1200 - 1500 cP | resin age: 6 months |
Hybrid Plastics Fireban® Mark VI Resorcinolinic (PRF) The resin system produces a superiour fire resistant material.Information provided by Hybrid Plastics |
|||
Brookfield Viscosity | 200 - 1500 cP | 200 - 1500 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4180 SBR Latex ROVENE® 4180 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is cross-linkable with external .. |
|||
Brookfield Viscosity | 200 - 1500 cP | 200 - 1500 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4306 SBR Latex ROVENE® 4306 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with outstanding strength properties. This self-crosslinking binder imparts excellent water and solvent r.. |
|||
Brookfield Viscosity | 200 - 1500 cP | 200 - 1500 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4487 SBR Latex ROVENE® 4487 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is cross-linkable with external .. |
|||
Brookfield Viscosity | 500 - 1500 cP | 500 - 1500 cP | #20/200 |
Mallard Creek Polymers Rovene® 6104 Resin Supported Emulsion Rovene® 6104 is a very soft, film forming vehicle that provides good water and rub resistance for flexographic and gravure inks and overprint varnishes. Rovene® 6104 can be used as the film fo.. |
|||
Brookfield Viscosity | 900 - 1500 cP | 900 - 1500 cP | Measured on 25% mass solution in toluene at 25°C; KM 06 |
Kraton® D1102 B (SBS) Liner Block Copolymer Description: Kraton D1102 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 29.5%. It is supplied from South America in the physical form identifie.. |
|||
Brookfield Viscosity | 550 - 1500 cP | 550 - 1500 cP | 15% MEK; MQSA 40A |
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane Pearlbond™ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo.. |
|||
Brookfield Viscosity | 900 - 1500 cP | 900 - 1500 cP | RVF #2 sp @ 20 rpm @ 80°F |
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information.. |
|||
Brookfield Viscosity | 1400 - 1500 cP @Temperature 23.9 °C |
1400 - 1500 cP @Temperature 75.0 °F |
Mixed, 1.5min |
BCC Products BC 8160 Urethane Casting BC8160 is a low viscosity two-component urethane casting compound that is specifically formulated for its flexural and impact strength. It is recommended for use for the production casting of highly.. |
|||
Brookfield Viscosity | 1400 - 1500 cP @Temperature 23.9 °C |
1400 - 1500 cP @Temperature 75.0 °F |
1.5 min mixed |
BCC Products BC 8860 Polyurethane Elastomer BC8860 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig.. |