Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.45 kN/m @Temperature -34.0 °C, Time 1.81e+6 sec |
14.0 pli @Temperature -29.2 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information.. |
|||
Peel Strength | 2.45 kN/m @Temperature 24.0 °C, Time 432000 sec |
14.0 pli @Temperature 75.2 °F, Time 120 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 5 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 5 is a sprayable contact adhesive which may be used to bond many high-pressure plastic laminates to wood, particle-board, metal and other surfacesInforma.. |
|||
Peel Strength | 2.45 kN/m @Time 259000 sec |
14.0 pli @Time 72.0 hour |
Adhesion to Truck Paint; ASTM D3330 |
3M 4411N Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 2.45 kN/m @Temperature 82.0 °C, Time 1.81e+6 sec |
14.0 pli @Temperature 180 °F, Time 504 hour |
180°, Canvas/Steel |
3M Fastbond™ 4213-NF Industrial Adhesive 3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when.. |
|||
Peel Strength | 2.45 kN/m @Temperature -34.0 °C, Time 1.81e+6 sec |
14.0 pli @Temperature -29.2 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 4799 Industrial Adhesive 3M™ Scotch-Weld™ Industrial Adhesive 4799 can be used to bond most EPDM rubber, sponge rubber, rubber sheeting, felt, canvas, linoleum and other lightweight materials to many metals, woods, concre.. |