Mechanical Properties Metric English Comments
Peel Strength 4.21 kN/m

@Temperature 80.0 °C
24.0 pli

@Temperature 176 °F
Floating Roller Peel
Hexcel® Redux® 610W (0.03 psf) Flame retarded epoxy film adhesive
Redux 610 is a modified, flame-retarded epoxy film adhesive curing at 250°F. It is suitable for bonding metal to metal and for sandwich structures where flame retardancy and low heat release are re..
Peel Strength 4.21 kN/m

@Temperature 60.0 °C,
Time 605000 sec
24.0 pli

@Temperature 140 °F,
Time 168 hour
JRF/SW, MIL-C-27725; AMS-S83318
3M AC-250 A-1/6 Aerospace Sealant
3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable l..
Peel Strength 4.21 kN/m

@Temperature 60.0 °C,
Time 605000 sec
24.0 pli

@Temperature 140 °F,
Time 168 hour
JRF/SW, Alclad; AMS-S83318
3M AC-250 A-1/6 Aerospace Sealant
3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable l..
Peel Strength 4.21 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
24.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive
3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat..
Peel Strength 4.21 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
24.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1357-L Neoprene High Performance Contact Adhesive
3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat..
Peel Strength 4.21 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
24.0 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive
Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information..
Peel Strength 4.21 kN/m

@Temperature 24.0 °C,
Time 432000 sec
24.0 pli

@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive
Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information..
Peel Strength 4.21 kN/m

@Temperature 24.0 °C,
Time 259000 sec
24.0 pli

@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
3M Fastbond™ 4213-NF Industrial Adhesive
3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when..
Peel Strength 4.21 kN/m

@Temperature 24.0 °C,
Time 259000 sec
24.0 pli

@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
3M Scotch-Weld™ 4475 Industrial Adhesive
Features: Dries quickly to a firm bondExcellent resistance to water, plasticizer migration, many detergent and soap solutions, oils and greasesA general purpose adhesive for bonding most vinyls, cer..
Copyright © lookpolymers.com All Rights Reserved