Isoflon PCTFE Polychlorotrifluoroethylene

Category Polymer , Thermoplastic , Fluoropolymer , Polychlorotrifluoroethylene (PCTFE); Molded
Manufacturer Isoflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PCTFE Polychlorotrifluoroethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluoropolymer material specifications.Information provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 2.10 - 2.16 g/cc
2.10 - 2.16 g/cc
ISO 12086
Water Absorption 0.00 %
0.00 %
DIN 53 495
Mechanical Properties Metric English Comments
Hardness, Shore D 72 - 80
72 - 80
DIN 53 505
Ball Indentation Hardness 65.0 - 70.0 MPa
9430 - 10200 psi
DIN 53 456
Tensile Strength 32.0 - 40.0 MPa
4640 - 5800 psi
DIN 53455
Elongation at Break 100 - 250 %
100 - 250 %
DIN 53455
Tensile Modulus 1.00 - 2.00 GPa
145 - 290 ksi
DIN 53457
Coefficient of Friction, Dynamic 0.35
0.35
on steel
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 20.0 - 100 °C
27.8 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 170 °C
338 °F
Continuous
Minimum Service Temperature, Air -273 °C
-459 °F
Continuous
Electrical Properties Metric English Comments
Dielectric Strength 50.0 - 70.0 kV/mm
1270 - 1780 kV/in
DIN 53481