Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.0 - 70.0 kV/mm | 280 - 1780 kV/in | Average value: 27.9 kV/mm Grade Count:55 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Dielectric Strength | 11.0 kV/mm @Thickness 3.17 mm |
280 kV/in @Thickness 0.125 in |
Unconditioned; ASTM D149 |
Garlock Bay State 22 Natural/SBR Sheet Rubber Blend of natural and SBR rubber, specially compounded to be quick-sealing, non-hardening and heat resistant.Red, smooth rotocured finish. It conforms easily to uneven flange surfaces.Information pr.. |
|||
Dielectric Strength | 11.0 kV/mm | 280 kV/in | short time 2 mm thick; ASTM D149 |
Saint-Gobain Meldin® 7021 CM Compression Molded Graphite Filled Polyimide Melidin® 7021 CM is a self-lubricating compression molded polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best fo.. |
|||
Dielectric Strength | 11.0 kV/mm @Thickness 3.00 mm |
280 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced Features: Heat Stabilized; Warp Resistant Forms: Pellets Additive: Heat Stabilizer Automotive Specifications: GM GMP.PA6.011Information Provided by Teknor Apex |
|||
Dielectric Strength | 11.0 kV/mm @Thickness 3.00 mm |
280 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi.. |
|||
Dielectric Strength | 11.0 kV/mm | 280 kV/in | ASTM D149 |
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent.. |
|||
Dielectric Strength | 11.0 kV/mm @Thickness 3.00 mm |
280 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S.. |
|||
Dielectric Strength | 11.0 kV/mm | 280 kV/in | ASTM D149 |
Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products
(discontinued **) Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin that has outstanding resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated s.. |
|||
Dielectric Strength | 11.0 - 80.0 kV/mm | 280 - 2030 kV/in | Average value: 23.9 kV/mm Grade Count:27 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |