Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCG20BK Copolymer PP, 20% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCG30BK Copolymer PP, 30% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCG40BK Copolymer PP, 40% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCM10BK Copolymer PP Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCM15BK Copolymer PP Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 232 °C | 300 - 450 °F | |
DuPont Nucrel® 535 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 535 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Melt Temperature | 149 - 232 °C | 300 - 450 °F | |
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Melt Temperature | 149 - 232 °C | 300 - 450 °F | |
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Melt Temperature | 149 - 232 °C | 300 - 450 °F | |
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2806 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Melt Temperature | 149 - 279 °C | 300 - 534 °F | Average value: 219 °C Grade Count:177 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Melt Temperature | 149 °C | 300 °F | |
Spartech E65050 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Melt Temperature | 149 - 232 °C | 300 - 450 °F | |
DuPont Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Melt Temperature | 149 - 232 °C | 300 - 450 °F | |
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC1390AA Low Density Polyethylene WESTLAKE low-density polyethylene EC1390 is used primarily in extrusion-coating applications that require fast line speeds and relatively low coating weights. When compared with other low-density po.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC1924AA Low Density Polyethylene WESTLAKE low-density polyethylene EC1924 is a resin that is widely used in the boardstock coating industry. This material has an excellent combination of low neck-in, ease of processing, good chill-.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC4041AA Low Density Polyethylene WESTLAKE low-density polyethylene EC4041 is recommended for use in the boardstock coating industry. The resin has low neck-in and good drawdown characteristics. Coatings produced from EC4041 have ex.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC4056AA Low Density Polyethylene WESTLAKE low-density polyethylene EC4056 is a natural low density material with an 80 melt index.FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All in.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC808AA Low Density Polyethylene WESTLAKE low-density polyethylene EC808 is a general-purpose formulation used for injection molding, general-purpose extrusion coating and laminating. It can be drawn down to low coating weights, is.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC811AA Low Density Polyethylene WESTLAKE low-density polyethylene EC811 is used for extrusion coating applications. It exhibits good adhesion, low coat weight, and fast heat seals.Application/UsesCoatings for paper/paperboardFDA: .. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EC850AA Low Density Polyethylene WESTLAKE low-density polyethylene EC850 is a resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density provides goo.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EM182AA Low Density Polyethylene WESTLAKE low-density polyethylene EM182 is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easi.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EM184AA Low Density Polyethylene WESTLAKE low-density polyethylene EM184 is a low density injection-molding formulation suggested for the production of closures where a high melt index is needed to meet shrinkage requirements and f.. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EM811AA Low Density Polyethylene WESTLAKE low-density polyethylene EM811 is a low-density polyethylene used for injection molding. It is characterized by high flow and low stiffness.Application/UsesFlexible medicalMedicalFDA: This .. |
|||
Melt Temperature | 149 - 166 °C | 300 - 330 °F | |
Westlake EM812AA Low Density Polyethylene WESTLAKE low-density polyethylene EM812 is a low-density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easi.. |
|||
Melt Temperature | 149 °C | 300 °F | |
Axiall 47551 Flexible PVC Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 149 - 232 °C | 300 - 450 °F | Average value: 193 °C Grade Count:3 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min.. |
|||
Melt Temperature | 149 - 310 °C | 300 - 590 °F | Average value: 221 °C Grade Count:81 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |
|||
Melt Temperature | 149 °C | 300 °F | |
Axiall 4750 Flexible PVC General purpose molding and extrusion compound well suited for automotive floor mats.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 149 - 204 °C | 300 - 400 °F | |
Ecomass® 5100TU96 Tungsten Filled SEBS Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled SEBS Base ResinVery FlexibleInformation provided by Technical.. |