Polymer Property : Melt Temperature = 191 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 191 - 196 °C
376 - 385 °F
PolyOne Geon™ Vinyl Flexible B8502 Polyvinyl Chloride, Flexible (PVC, Flexible)
A flexible PVC Compound with good resistance to migration to specific applications.Information provided by PolyOne
Melt Temperature 191 - 210 °C
376 - 410 °F
Average value: 203 °C Grade Count:11
Overview of materials for Chlorinated PVC (CPVC)
This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr..
Melt Temperature 191 °C
375 °F
Blown
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
Melt Temperature 191 °C
375 °F
Teknor Apex APEX® 3210-90 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Melt Temperature 191 °C
375 °F
Teknor Apex APEX® 3211-90 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Melt Temperature 191 °C
375 °F
Teknor Apex APEX® 82-E211-B Polyvinyl Chloride, Flexible
Notes: 80°C Insulation; RoHS Compliant Uses: Transportation Wire Insulation Agency Ratings: SAE J1128 Automotive Specifications: Chrysler MS-DC16 Type A Processing Method: Extrusion Forms: Pell..
Melt Temperature 191 °C
376 °F
DuPont™ Surlyn® 1650 Zinc Ionomer Resin for Blown and Cast Film
Surlyn® 1650 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Melt Temperature 191 - 204 °C
375 - 400 °F
Clariant CA9000NAT` Acetal Copolymer
Data provided by Clariant Masterbatches
Melt Temperature 191 - 221 °C
375 - 430 °F
Clariant Renol PP1100N40CC Polypropylene Homopolymer, 40% Glass Fiber and Mineral Reinforced, Chemically Coupled
Data provided by Clariant Masterbatches
Melt Temperature 191 °C
375 °F
Axiall 4510 Flexible PVC
Non-lead stabilized 105C rated automotive harness compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 191 °C
375 °F
Axiall 19482 Wire & Cable Flexible PVC
105°C, VW-1 rated non-lead stabilized insulation compound. Ideally suited for 18 AWG, 1/64 wall. UL approved for TW, THW, THHW applications.Information provided by Georgia GulfGeorgia Gulf became..
Melt Temperature 191 °C
376 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 22% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 191 °C
376 °F
Injection
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 22% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Melt Temperature 191 °C
375 °F
Axiall 4501 Flexible PVC
Non-lead stabilized, 105C rated automotive harness compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Melt Temperature 191 °C
375 °F
Axiall 4470 Flexible PVC
High speed ultrathinwall automotive harness wire per SAE J1128.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.