Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible Y126 White 317 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne LubriOne™ ATH-000/18T 2S Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 193 - 221 °C | 379 - 430 °F | |
PolyOne Edgetek® PE-30GF/000 Polyethylene, High Density (HDPE) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ HTX L1502 Polyvinyl Chloride Alloy (PVC Alloy) Physical properties based on Geon HTX L1502 white 1000.Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Dry Blend E7364 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 193 - 210 °C | 379 - 410 °F | |
PolyOne Geon™ Vinyl Dry Blend E7755 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible A4DU5 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible A6DE3 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible A8001 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible A8501 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible B7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 199 °C | 379 - 390 °F | |
PolyOne Geon™ Vinyl Flexible B85UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible B9WF1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible R132BE Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible R235AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 210 °C | 379 - 410 °F | |
PolyOne Geon™ Vinyl Flexible R290AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 °C | 379 °F | |
Chevron Phillips 1124 Liner Grade Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Good Impact Strength, Good Processability, Low Gels, Good Sealability, Medium Slip, High AntiblockApplications:Trash Bags and other LinersProcessing Condition.. |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible C5D01 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 199 °C | 379 - 390 °F | |
PolyOne Geon™ Vinyl Flexible C7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible G92B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible R264AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 216 °C | 379 - 421 °F | Stock |
PolyOne Lubri-Tech™ AT-15GP/05T Acetal With Graphite - 5% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 193 - 232 °C | 379 - 450 °F | Injection |
Chevron Phillips K-Resin® BK12 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: BK12 is an SBC consisting of KR01 grade with a mold release added for easier processing. BK12 molded parts give excellent detail on fast production cyc.. |
|||
Melt Temperature | 193 °C | 379 °F | Blown Film |
Westlake EF528 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF528 is an ethylene vinyl acetate copolymer with 18.5% VA. EF528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength .. |
|||
Melt Temperature | 193 - 210 °C | 379 - 410 °F | Extrusion |
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Temperature | 193 - 210 °C | 379 - 410 °F | Molding |
Lubrizol Estane® 2103-90AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Temperature | 193 - 210 °C | 379 - 410 °F | Molding |
Lubrizol Estane® 2103-90AEFH Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
Melt Temperature | 193 - 232 °C | 379 - 450 °F | Injection |
Chevron Phillips K-Resin® BK10 Styrene-Butadiene Copolymer, Injection Molding Grade Styrene-Butadiene CopolymerCustomer Benefits: BK10 is an SBC developed specifically to have enhanced flow capabilities. It offers improved processability and lower cycle times with the optical clar.. |
|||
Melt Temperature | 193 - 232 °C | 379 - 450 °F | Injection |
Chevron Phillips K-Resin® BK13 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerBK13 is an SBC developed specifically to have enhanced flow capabilities and improved stiffness over the KR01 grade. BK13 molded parts give excellent detail on rapid prod.. |
|||
Melt Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne LubriOne™ ATH-05KV/000 Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |