Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 227 - 238 °C | 441 - 460 °F | |
PolyOne Stat-Tech™ AS-1000 AS Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Melt Temperature | 227 - 238 °C | 441 - 460 °F | |
PolyOne Stat-Tech™ AS-13CF/000 Black Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Melt Temperature | 227 - 238 °C | 441 - 460 °F | |
PolyOne Trilliant™ HC HC7300-0013 ESD Black Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Melt Temperature | 227 - 232 °C | 441 - 450 °F | |
Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Melt Temperature | 227 - 232 °C | 441 - 450 °F | |
Chevron Phillips Vytek™ V205E9 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Melt Temperature | 227 - 232 °C | 441 - 450 °F | |
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Melt Temperature | 227 - 232 °C | 441 - 450 °F | |
Chevron Phillips Vytek™ V208C3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Melt Temperature | 227 - 232 °C | 441 - 450 °F | |
Chevron Phillips Vytek™ V208C6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Melt Temperature | 227 - 232 °C | 441 - 450 °F | |
Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart drop impact, hot-tack and heat seal properties, good drawdown, can b.. |
|||
Melt Temperature | 227 °C | 441 °F | pyrometer check of air shot |
Lubrizol ESTAGRIP® ST70A Polyether-Type Thermoplastic Polyurethane Features: Low durometer soft feel for excellent grip; outstanding adhesionUses: Injection Molding - OvermoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation provided.. |
|||
Melt Temperature | 227 °C | 441 °F | pyrometer check of air shot |
Lubrizol ESTAGRIP® ST80A Polyether-Type Thermoplastic Polyurethane Features: Low durometer soft feel for excellent grip; outstanding adhesionUses: Injection Molding - OvermoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation provided.. |
|||
Melt Temperature | 227 °C | 441 °F | |
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol |
|||
Melt Temperature | 227 °C | 441 °F | |
Lubrizol Estaloc® 59020 Reinforced Thermoplastic Polyurethane Type: Estaloc® 59020 RETPU is a polyester-type reinforced engineered thermoplastic polyurethane (RETPU).Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.. |
|||
Melt Temperature | 227 °C | 441 °F | |
Lubrizol ESTALOC® 59104 Ester-Type, Reinforced Engineering Thermoplastic Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impactUses: Injection Molding Available in Americas and AsiaInformation provided by Lubrizol |
|||
Melt Temperature | 227 °C | 441 °F | |
Lubrizol ESTALOC® 60204 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Melt Temperature | 227 °C | 441 °F | |
E-Polymers SEPAZ® N4040M2 Dimensional Stability Heat Resistance Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Melt Temperature | 227 - 235 °C | 441 - 455 °F | |
LNP Thermocomp® SF-1006 Polyamide 12, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Melt Temperature | 227 - 260 °C | 441 - 500 °F | |
LNP Thermocomp® HF-1006 Polyamide 11, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Melt Temperature | 227 - 232 °C | 441 - 450 °F | |
Chevron Phillips Vytek™ V208A3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Melt Temperature | 227 °C | 441 °F | |
E-Polymers SEPAZ® N4040M1 Dimensional Stability Heat Resistance Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |