Material Notes:
Mxsten CV Plastomer CV77516 resin is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock additives. Films produced with this resin exhibit a very low seal initiation temperature with a broad hot tack window. Other features of this resin include higher stiffness and high melting point.Application/UsesBlown filmFood packagingFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D1505
Thickness 25.4 microns
1.00 mil
Melt Flow 1.0 g/10 min
1.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 750 %
750 %
ASTM D882
Film Elongation at Break, TD 1050 %
1050 %
ASTM D882
Dart Drop 66.9 g/micron
1700 g/mil
ASTM D1709A
Film Tensile Strength at Break, MD 56.5 MPa
8200 psi
ASTM D882
Film Tensile Strength at Break, TD 44.1 MPa
6400 psi
ASTM D882
Heat Seal Strength Initiation Temperature 88.0 °C
190 °F
Westlake
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ASTM D1003
Gloss 60 %
60 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 216 - 232 °C
420 - 450 °F
Blow-up Ratio (BUR) 2.4
2.4
Descriptive Properties Value Comments
Process Blown Film
Film
Region US & Canada
Bamberger Polymers Distribution