Polymer Property : Melt Temperature = 215 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 195 - 215 °C
383 - 419 °F
SABIC 118 Series Linear Low Density Polyethylene for Blown Film
Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st..
Melt Temperature 195 - 215 °C
383 - 419 °F
SABIC 120W Linear Low Density Polyethylene for Blown Film
Product Description: 120W is a Linear Low Density Polyethylene grade suitable for general purpose packaging. Films produced using this resin yield good tensile properties, impact strength and opti..
Melt Temperature 170 - 215 °C
338 - 419 °F
Recommended
NOVA Chemicals Sclair® 19C (High Gloss) HDPE Blow Molding Resin
19C complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te..
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin
Features: High stiffness, high impact strength and low warpage, good top loading capability, high surface gloss.Applications: Container (tub) lids and closures.Data provided by the manufacturer.
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 2908C HDPE Injection Molding Resin
High stiffness, Maximum impact strength and toughnessApplications: Tote boxes, Beverage cratesAdditives: AntioxidantInformation provided by NOVA Chemicals.
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 2909 HDPE Injection Molding Resin
High stiffness, Maximum impact strength and toughness, Good top loading capability, High surface glossApplications: Tote boxes, Beverage cratesAdditives: Antioxidant, Ultraviolet light stabilizersIn..
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 56B4 HDPE Blow Molding Resin
Extra-high stress crack resistance, Good processabilityApplications: Very high ESCR, Ideally suited for use in most food, pharmaceutical, households and industrial chemical applications, Little/no s..
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 8111 LLDPE Injection Molding Resin  (discontinued **)
Features: Good processability, excellent impact resistance, excellent flexibility and freedom from warpage.Applications: Automotive splash-guards, large containers, closures and lids for food applic..
Melt Temperature 195 - 215 °C
383 - 419 °F
LATI LASTANE 50 High Impact Polyurethane (PUR)  (Unverified Data**)
Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper..
Melt Temperature 20.0 - 215 °C
68.0 - 419 °F
Average value: 184 °C Grade Count:30
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 2607 HDPE Injection Molding Resin
Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer.
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 2508-UV9 MDPE Injection Molding Resin  (discontinued **)
Features: Excellent processability for applications requiring stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids.Data provided by the manufacturer.
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 8405 UV8D, 8405G UV8D MDPE Rotational Molding Resin  (discontinued **)
Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer.
Melt Temperature 175 - 215 °C
347 - 419 °F
DuPont Elvax® 3190 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..
Melt Temperature 175 - 215 °C
347 - 419 °F
Blown/Cast Film Coextrusion
DuPont™ Elvax® 3190A Ethylene Vinyl Acetate
DuPont™ Elvax® 3190A is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3..
Melt Temperature 190 - 215 °C
374 - 419 °F
Injection-molding
BASF Ultraform® N2650 Z4 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr..
Melt Temperature 190 - 215 °C
374 - 419 °F
Injection-molding
BASF Ultraform® N2650 Z2 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr..
Melt Temperature 175 - 215 °C
347 - 419 °F
Huntsman Rexell® V8402 Cast Film Extrusion LLDPE  (discontinued **)
Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent mechanical strength, low sealing temperature, and good flex crack resistanceApplications: Sealing layer in..
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 2607-UV9 HDPE Injection Molding Resin  (discontinued **)
Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer.
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 2514 MDPE Injection Molding Resin  (discontinued **)
Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids, housewares, deep skirt lids,..
Melt Temperature 170 - 215 °C
338 - 419 °F
NOVA Chemicals Sclair® 8306 BK, 8306G BK MDPE Rotational Molding Resin  (discontinued **)
Features: Balanced combination of toughness, ESCR and processability.Applications: General purpose.Data provided by the manufacturer.
Melt Temperature 182 - 215 °C
360 - 419 °F
ExxonMobil Santoprene® 8271-80HT Thermoplastic Rubber  (discontinued **)
Description: A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use. It can be processed using injection molding or extrusion melt pro..
Melt Temperature 190 - 215 °C
374 - 419 °F
Injection molding
BASF Ultraform® N2650 Z6 POM + PUR
Description: Elastomer-modified injection molding grade for applications requiring highest impact strength together with low stiffness.Information provided by BASF
Melt Temperature 175 - 215 °C
347 - 419 °F
DuPont Elvax® 3190LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion  (discontinued **)
25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..
Melt Temperature 175 - 215 °C
347 - 419 °F
DuPont Elvax® 3175LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion  (discontinued **)
28 wt% Vinyl Acetate.Elvax® 3175 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..
Melt Temperature 204 - 215 °C
399 - 419 °F
Huntsman PE1451 EVA Film Extrusion  (discontinued **)
4.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Melt Temperature 190 - 215 °C
374 - 419 °F
Injection molding
BASF Ultraform® N2644 Z9 POM + PUR
Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.Information provided by BASF