Material Notes:
High Specific GravityStainless Steel/Tungsten Powder Filled ABSInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 6.00 g/cc
6.00 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 16.5 MPa
2400 psi
ASTM D638
Elongation at Break 1.1 %
1.1 %
ASTM D638
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 204 - 249 °C
400 - 480 °F
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
Drying Temperature 71.1 - 82.2 °C
160 - 180 °F
Dry Time 2 - 4 hour
2 - 4 hour