Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Drying Temperature | 76.7 °C | 170 °F | |
RTP Company RTP 6003-55A Z Specialty Thermoplastic Elastomer, Bondable to PC/PMMA, PC/PBT |
|||
Drying Temperature | 76.7 °C | 170 °F | |
RTP Company RTP 6003-75A Z Specialty Thermoplastic Elastomer, FDA Compliant Ingredients |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/10/E Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/10/FR Polypropylene Homopolymer, 10% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/20/FR Polypropylene Homopolymer, 20% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/20/H Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/30/E/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/40 Polypropylene Homopolymer, 40% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-60/40/E8 Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® PP-15/T/10/20 Polypropylene Homopolymer, 22% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 - 93.3 °C | 170 - 200 °F | 4 to 24 hrs; Tray Dryer |
Shuman 730 Utility White ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the Shuman Plastics, Inc. |
|||
Drying Temperature | 76.7 °C @Time 7200 sec |
170 °F @Time 2.00 hour |
|
RTP Company RTP 2700 S-60A MD NATURAL Saturated Styrenic Block Copolymer ISO 10993 Tested ISO 10993 is used to evaluate the biocompatibility of medical devices. Consult RTP Company for more details. |
|||
Drying Temperature | 76.7 °C | 170 °F | |
RTP Company RTP 2700 S-60A Z Saturated Styrenic Block Copolymer, FDA Compliant Ingredients |
|||
Drying Temperature | 76.7 °C @Time 7200 sec |
170 °F @Time 2.00 hour |
|
RTP Company RTP 2700 S-70A MD NATURAL Saturated Styrenic Block Copolymer ISO 10993 Tested ISO 10993 is used to evaluate the biocompatibility of medical devices. Consult RTP Company for more details. |
|||
Drying Temperature | 76.7 °C | 170 °F | |
RTP Company RTP 2700 S-80A Z Saturated Styrenic Block Copolymer (TES/SEBS or other), FDA Compliant Ingredients |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-62/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PPX-FR4 Modified PPO, UL 94 V-1 with HDT of 185 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Fiberfil® J-68/30/E/UV Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Drying Temperature | 76.7 °C | 170 °F | |
RTP Company RTP 2700 S-70A Z Saturated Styrenic Block Copolymer, FDA Compliant Ingredients |