Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Drying Temperature = 170 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 76.7 °C
170 °F
PolyOne Gravi-Tech™ GRV-TP-080-W-NAT Styrene Butadiene Block Copolymer (SBC)
Information provided by PolyOne
Drying Temperature 76.7 - 82.2 °C
170 - 180 °F
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 76.7 - 82.2 °C
170 - 180 °F
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant
PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
Drying Temperature 76.7 - 82.2 °C
170 - 180 °F
Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced
PC/ABS Alloy, Flame Retardant, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
Drying Temperature 76.7 - 82.2 °C
170 - 180 °F
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow
PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by ..
Drying Temperature 76.7 °C

@Time 7200 - 14400 sec
170 °F

@Time 2.00 - 4.00 hour
RTP Company RTP 6003-75A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested
Drying Temperature 76.7 °C
170 °F
RTP Company RTP 6003-75A Z Specialty Thermoplastic Elastomer, FDA Compliant Ingredients
Drying Temperature 76.7 - 82.2 °C
170 - 180 °F
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade
PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
Drying Temperature 76.7 - 82.2 °C
170 - 180 °F
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade
PC/ABS Alloy, General Purpose, Low Gloss GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid..
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® J-60/20 Polypropylene Homopolymer, 20% Glass Reinforced
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® J-60/30/E Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® M-1492 BK223 Polypropylene Homopolymer, Glass Reinforced, mica Filled, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® M-1812 Polypropylene Homopolymer, 45% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® PP-60/TC/24/D/HS Polypropylene Homopolymer, Talc Filled, Heat Stabilized
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® J-60/15/MI/20 Polypropylene Homopolymer, 35% Glass/mica Reinforced
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® J-60/20/E8/M Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® J-62/30/E8 Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 - 87.8 °C
170 - 190 °F
Star Plastics ABS450FR Molding Grade ABS
Information provided by Star Plastics, Inc.
Drying Temperature 76.7 °C
170 °F
RTP Company RTP 2700 S-60A Z Saturated Styrenic Block Copolymer, FDA Compliant Ingredients
Drying Temperature 76.7 °C

@Time 7200 sec
170 °F

@Time 2.00 hour
RTP Company RTP 2700 S-70A MD NATURAL Saturated Styrenic Block Copolymer ISO 10993 Tested
ISO 10993 is used to evaluate the biocompatibility of medical devices. Consult RTP Company for more details.
Drying Temperature 76.7 °C

@Time 7200 - 14400 sec
170 °F

@Time 2.00 - 4.00 hour
RTP Company RTP 2740 S-60A Saturated Styrenic Block Copolymer General Purpose
Drying Temperature 76.7 - 82.2 °C
170 - 180 °F
Polymer Resources PPX-FR2 Modified PPO, UL 94 V-1 with HDT of 210 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 76.7 °C
170 °F
PolyOne Gravi-Tech™ GRV-TP-050-CU-NAT Styrene Butadiene Block Copolymer (SBC)
Information provided by PolyOne
Drying Temperature 76.7 °C
170 °F
Drying not normally required
Fiberfil® J-68/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Drying Temperature 76.7 °C
170 °F
RTP Company RTP 2700 S-70A Z Saturated Styrenic Block Copolymer, FDA Compliant Ingredients
Copyright © lookpolymers.com All Rights Reserved