Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 82.2 °C | 180 °F | |
PolyOne Nymax™ GF 1200 33 Red 31 A Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
PolyOne Nymax™ GMF 604 40 UV Black 148 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Drying Temperature | 82.0 °C | 180 °F | Desiccant drying for 3 hours recommended |
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and c.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
ExxonMobil Santoprene® 201-68W228 Thermoplastic Elastomer
(discontinued **) A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated for low density foamed profile extrusion applications and has lon.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Drying Temperature | 82.0 °C | 180 °F | |
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
PolyOne Nymax™ ND633 GF Natural Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
PolyOne Nymax™ X GMF 604 40 UV Black 148 rev 4 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 405 Polystyrene (PS), Glass Fiber |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 600 HB Acrylonitrile Butadiene Styrene (ABS), UL94 HB |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 603 Acrylonitrile Butadiene Styrene (ABS), Glass Fiber |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 603 TFE 15 Acrylonitrile Butadiene Styrene (ABS), Glass Fiber - PTFE Lubricated |
|||
Drying Temperature | 82.2 °C @Time 14400 sec |
180 °F @Time 4.00 hour |
|
RTP Company RTP 6091-85A PA12 BLACK Specialty Thermoplastic Elastomer, PA-12 bondable - manufactured with Santoprene™ TPV technology |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 661 Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber - EMI/RFI/ESD Protection |
|||
Drying Temperature | 82.2 °C @Time 14400 sec |
180 °F @Time 4.00 hour |
|
RTP Company VLF 80111 CC Polypropylene (PP), Long Glass Fiber - Chemically Coupled |
|||
Drying Temperature | 82.2 °C | 180 °F | Average value: 82.2 °C Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled 13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Drying Temperature | 82.0 - 85.0 °C | 180 - 185 °F | |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
Teknor Apex Sarlink® 3190 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3190 can be processed by blow molding, injection molding or.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 299 A X 108950 H Nylon 6 (PA), High Gravity Compound |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 1200 T-80A Ether-based Thermoplastic Polyurethane Elastomer |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 207 A TFE 13 SI 2 Nylon 6 (PA), Glass Fiber - PTFE Lubricated - Silicone Lubricated |
|||
Drying Temperature | 82.2 °C | 180 °F | do not over dry |
Ecomass® 4703BI74 Filled Polyurethane, Injection Molding Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, radiation shielding applicationsInfor.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
ExxonMobil Santoprene® 241-64 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
Celanese Celcon® CFX-0308 PTFE and Silicone Modified Acetal Copolymer Description: CFX-0308 is a general purpose acetal copolymer modified with PTFE and silicone fluid for low friction in sliding andor wear applications.Information provided by Celanese Corporation. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
ExxonMobil Santoprene® 211-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(disconti Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |