Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 82.2 °C | 180 °F | |
PolyOne Nymax™ GB 1200 20 HS BLACK 18 Polyamide 66 (Nylon 66) Preliminary Data SheetMolded Test Bars: Dry as MoldedInformation provided by PolyOne |
|||
Drying Temperature | 82.2 °C | 180 °F | |
PolyOne Nymax™ GB 1200 30 HS BLACK 18 Polyamide 66 (Nylon 66) Preliminary Data SheetMolded Test Bars: Dry as MoldedInformation provided by PolyOne |
|||
Drying Temperature | 82.2 °C | 180 °F | |
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
PolyOne Nymax™ GF 1200 A 13 Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
PolyOne Nymax™ GF 1200 A 33 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
PolyOne Nymax™ GF 1200 A 43 Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 400 TFE 5 Polystyrene (PS), PTFE Lubricated |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 4605 FR Syndiotactic Polystyrene (SPS), Glass Fiber - Flame Retardant |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 4607 FR Syndiotactic Polystyrene (SPS), Glass Fiber - Flame Retardant |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 600 GB 10 Acrylonitrile Butadiene Styrene (ABS), Glass Bead |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 603 Acrylonitrile Butadiene Styrene (ABS), Glass Fiber |
|||
Drying Temperature | 82.2 °C @Time 7200 - 14400 sec |
180 °F @Time 2.00 - 4.00 hour |
|
RTP Company RTP 6042-70A Specialty Thermoplastic Elastomer, PC/ABS Bondable |
|||
Drying Temperature | 82.2 °C | 180 °F | |
PolyOne Edgetek® 5209 Black 30 A 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
PolyOne Edgetek® NL-30GF/000 FR Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
MTI ThermoStran® TPU-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Star Plastics ABS3030 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass Information provided by Star Plastics, Inc. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
Teknor Apex Sarlink® 4490 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4490 is a medium hardness grade possessing exceptional tensile strength, superior compressio.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company ESD C 680 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber - ESD Protection - Electrically Conductive |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 200 A TFE 15 Nylon 6 (PA), PTFE Lubricated |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP 299 A X 108950 D Nylon 6 (PA), High Gravity Compound |
|||
Drying Temperature | 82.2 °C | 180 °F | |
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Drying Temperature | 82.2 °C | 180 °F | |
PolyOne Edgetek® AT-25GF-10MN/000 BLASCK Acetal-Copolymer, Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 82.2 °C @Time 7200 sec |
180 °F @Time 2.00 hour |
|
RTP Company RTP 283 A Nylon 6 (PA); Carbon Fiber |
|||
Drying Temperature | 82.2 °C | 180 °F | |
LNP Thermotuf® QF-1006 HI Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
(discontinued **) Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades .. |
|||
Drying Temperature | 82.2 °C @Time 7200 sec |
180 °F @Time 2.00 hour |
|
RTP Company RTP 205 A HI Nylon 6 (PA), Glass Fiber - Impact Modified |
|||
Drying Temperature | 82.2 °C | 180 °F | |
RTP Company RTP PA6 30 GF NAT Nylon 6 (PA), Value Product - Glass Fiber - Heat Stabilized |