Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 82.0 - 116 °C | 180 - 241 °F | |
Styron EMERGEâ„¢ 4702-15 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
Mold Temperature | 82.0 - 104 °C | 180 - 219 °F | |
Elastocon TPE Technologies Elastocon® STK56PA Thermoplastic Elastomer Elastocon® STK56PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA is well suited for consumer go.. |