E-Polymers Tekaloy® G70GR , 30% Glass Reinforced PC/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Glass Fiber Filled , Polycarbonate (PC)
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKALOY®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers Tekaloy® G70GR , 30% Glass Reinforced PC/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Fiber reinforced, High stiffness, Dimensional stabilityInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 105 MPa
15200 psi
ASTM D638
Elongation at Break 3.2 %
3.2 %
ASTM D638
Flexural Yield Strength 155 MPa
22500 psi
ASTM D790
Flexural Modulus 7.20 GPa
1040 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 230 - 300 °C
446 - 572 °F
Mold Temperature 70.0 - 110 °C
158 - 230 °F