Processing Properties Metric English Comments
Mold Temperature 40.6 - 71.1 °C
105 - 160 °F
Ravago Manufacturing Americas Hylac® FR134 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Mold Temperature 40.6 - 71.1 °C
105 - 160 °F
Ravago Manufacturing Americas Hylac® FR74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Mold Temperature 40.6 - 79.4 °C
105 - 175 °F
Injection Molding
Styrolution Luran® S 778 T ASA
Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Mold Temperature 40.6 - 79.4 °C
105 - 175 °F
DuPont Surlyn® SG201U NC010 Supergloss Molding Alloy
Surlyn® SG201U is a modified ionomer resin for applications that require a high gloss, molded in color surface color surface finish directly from the mold. The material is weatherable, durable, an..