Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 230 - 240 °C | 446 - 464 °F | Average value: 235 °C Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Die Temperature | 200 - 240 °C | 392 - 464 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1047D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Die Temperature | 200 - 240 °C | 392 - 464 °F | Extrusion Molding |
LG Chemical KEYFLEX BT GN7142F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Low ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® IG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion Molding |
LG Chemical LUPOL GP1007FE Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Die Temperature | 210 - 240 °C | 410 - 464 °F | |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Die Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay TECHNYL® eXten D 458P PA6.10, DRY Description: Product in development - provisional datasheet. High viscosity unfilled plasticized PA6.10 for extrusion applications providing low end part warpage.Available in: Asia Pacific, Europe, .. |
|||
Die Temperature | 230 - 240 °C | 446 - 464 °F | |
Borealis Borcoat™ EA165E Elastomer Modified Polypropylene for Extrusion Borcoat EA165E is an elastomer modified compound, based on a high molecular weight copolymer. The elastomer modification gives excellent low temperature impact resistance.Borcoat EA165E is recommen.. |
|||
Die Temperature | 230 - 240 °C | 446 - 464 °F | |
Borealis Borcoat™ ME0420 Grafted Polyethylene Adhesive for Steel Pipe Coating Borcoat ME0420 is a maleic-anhydride grafted polyethylene polymer to be extruded on conventional LDPE extruders with flat die or crosshead and it has excellent adhesion to epoxy powder and the top c.. |
|||
Die Temperature | 230 - 240 °C | 446 - 464 °F | (6) Extrusion |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Die Temperature | 230 - 240 °C | 446 - 464 °F | (7) Tip, Extrusion |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Die Temperature | 190 - 240 °C | 374 - 464 °F | Hotmelt Coating Slot Die |
EMS-Griltech Griltex® D 1619E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | |
Arkema Group OREVAC® 18365-S Grafted Maleic Anhydride Polyethylene OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | |
Arkema Group OREVAC® 18510 Grafted Maleic Anhydride Polyethylene OREVAC 18510 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510 is mainly used in pipe .. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | |
Arkema Group OREVAC® 18760 Grafted Maleic Anhydride Polypropylene OREVAC 18760 is a maleic anhydride grafted polypropylene used in the manufacturing of three layer PP coating for steel pipeline. OREVAC 18760 is also used in multilayer EVOH – PP structures. OREVAC.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | |
Arkema Group OREVAC® PPC Grafted Maleic Anhydride Polypropylene OREVAC PPC is a grafted maleic anhydride polypropylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC PPC is mainly used in multi-layer tube to have good adhesion between PP, PA.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Average value: 230 °C Grade Count:3 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |