Description: Product in development - provisional datasheet. High viscosity unfilled plasticized PA6.10 for extrusion applications providing low end part warpage.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: Polyamide 6,10 for extrusion, where high flexibility and toughness are requested, especially low temperature toughness. TECHNYL® eXten D 458P is specially developed for automotive and other applications where a long term high temperature usage is requested. This material is available in black and natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527 Type 1A
Elongation at Break 150 %
150 %
ISO 527 Type 1A
Tensile Modulus 0.800 GPa
116 ksi
ISO 527 Type 1A
Flexural Strength 30.0 MPa
4350 psi
ISO 178
Flexural Modulus 0.690 GPa
100 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
8.70 J/cm²

@Temperature 23.0 °C
41.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ISO 11357
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
ISO 1210
HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
ISO 1210
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
ISO 1210
Processing Properties Metric English Comments
Feed Temperature 215 - 225 °C
419 - 437 °F
Front Barrel Temperature 225 - 235 °C
437 - 455 °F
Die Temperature 230 - 240 °C
446 - 464 °F
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Compression Zone 225-235°C