Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group OREVAC® 18760 Grafted Maleic Anhydride Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Arkema
Trade Name OREVAC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group OREVAC® 18760 Grafted Maleic Anhydride Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OREVAC 18760 is a maleic anhydride grafted polypropylene used in the manufacturing of three layer PP coating for steel pipeline. OREVAC 18760 is also used in multilayer EVOH – PP structures. OREVAC 18760 is mainly used in pipe coating to have good adhesion performances between an epoxy primer and a PP or between EVOH and PP for heating tube applications. OREVAC 18760 combined with a proper PP and epoxy fulfill the requirement of different application standards when applied in the rules of art.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ISO 1183
Melt Index of Compound 3.8 g/10 min

@Load 2.16 kg,
Temperature 210 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 410 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ISO 608
Tensile Strength at Break 43.0 MPa
6240 psi
ASTM D527-2
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO R 527-2
Elongation at Break 540 %
540 %
ISO R 527-2
Thermal Properties Metric English Comments
Melting Point 152 °C
306 °F
DSC
Vicat Softening Point 126 °C

@Load 0.999 kg
259 °F

@Load 2.20 lb
ISO 306
Processing Properties Metric English Comments
Zone 1 190 - 210 °C
374 - 410 °F
Zone 2 195 - 220 °C
383 - 428 °F
Zone 3 200 - 225 °C
392 - 437 °F
Zone 4 205 - 230 °C
401 - 446 °F
Die Temperature 220 - 240 °C
428 - 464 °F
Users viewing this material also viewed the following: